Fig. 3. (Color online) The deposition thicknesses of the SrRuO3 thin film deposited for (a) 5 minutes and (b) 50 minutes measured using a Transmission Electron Microscope.
New Phys.: Sae Mulli 2022;72:754~760 https://doi.org/10.3938/NPSM.72.754